| ID-MARK aluminum sheets and polyester overlam films were subjected to the following controlled and industry accepted test conditions. Results for each test are as indicated. These results are typical values; not to be used for specification use. |
| |
| CHEMICAL RESISTANCE |
TEST CONDITIONS |
RESULTS |
| Four hour immersion at room temperature in: |
|
| Water |
No Effect |
| Alcohol (Isopropyl) |
No Effect (w/overlam)
Slight Fading
(w/o overlam) |
| Oil |
No Effect |
| Hydrocarbons |
No Effect |
| Base (pH=10) |
No Effect |
| Acid (pH=4) |
No Effect |
|
| |
| ABRASION RESISTANCE |
TEST CONDITIONS |
RESULTS |
| Taber abraser CS-17 wheels with 1000g load: |
|
| With overlam |
700 cycles |
| Without overlam |
73 cycles |
|
| |
SALT
SPRAY
|
TEST CONDITIONS |
RESULTS |
| 5% concentration at 95° F |
No Effect (w/overlam) |
|
| |
|
EXTERIOR DURABILITY
|
TEST CONDITIONS |
RESULTS |
Humidity
95% relative humidity at 90° F
for 72 hours |
No Effect |
Temperature
-20° F + 250° F for 7 days |
No Effect |
Long-Term Exposure
5-year exposure at 90 degree angle on aluminum plates. Weatherometer simulated conditions |
Black: No Effect
Red (w/overlam): No Effect
Blue w/overlam): No Effect |
Shelf Life
Plates should be stored in a clean, low humidity area. Temperature should be 80° F or less. |
1 year |
|
| |
|
ID-MARK metal sheets meet the physical property requirements of MIL-P-15024D
|
|